application
high activity pop with solid content of 27 is used in preparation of high-load flexible polyurethane foam by mixing with high activity ppg. the hardening capability is higher than pop 36/28, but is less than hpop 40.
feature
high activity pop with solid content of 27 is used in preparation of high-load flexible polyurethane foam by mixing with high activity ppg. the hardening capability is higher than pop 36/28, but is less than hpop 40.
performance
hydroxylvalue(mgkoh/g) 23-27 water content(%)≤ 0.05 ph 5-8 viscosity(mpa·s/25℃)≤ 3500 functionality 3