polyether polyol can be used to produce high resilience slabstock foam.
feature
with a functionality of 3, molecular weight of 6000 super low ordor. content of primary hydroxyl reaches 85%, 90% lower in voc comparing with ep-3600, as well as the better activity and ablity of open-cell. fit for sponge material requires low ordor and low voc.
performance
hydroxylvalue(mgkoh/g)26.0-30.0 acid value(mgkoh/g)≤ 0.05 water content(%)≤ 0.05 unsaturatedvalue (mol/kg)≤ 0.08 viscosity (mpa·s/25℃)1060-1260 k (mg/kg)≤3 colourity(apha)≤50 functionality 3 molecular weight 6000